Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 11.98 MPa | 1737 psi | After oven air again 168 hrs. @ 150°C; ASTM D412 |
Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Tensile Strength at Break | 11.98 MPa | 1737 psi | AVG; ASTM D412 Method A |
Seals Eastern 5725 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |