Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 11.98 MPa
1737 psi
After oven air again 168 hrs. @ 150°C; ASTM D412
Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber  (discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
Tensile Strength at Break 11.98 MPa
1738 psi
AVG; ASTM D412 Method A
Seals Eastern 5514 Polyacrylate Rubber
General purpose Natural RubberInformation provided by Seals Eastern, Inc.
Tensile Strength at Break 11.98 MPa
1737 psi
AVG; ASTM D412 Method A
Seals Eastern 5725 Fluorocarbon-Elastomer
Formulated Viton®. General service.Information provided by Seals Eastern, Inc.