Polymer Property : Tensile Strength at Break = 167000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 1150 MPa
167000 psi
ThyssenKrupp SECURE 400 Structural Steel
This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 400 for civil use, this is usually produced in thickness from 3 mm up to 50 mm.App..