Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1140 MPa | 165000 psi | |
Goodfellow Nickel 55/Titanium 45 Shape Memory Alloy Shape memory alloy is a description applied to that group of metallic materials which show the ability to return to the previously defined shape or size when subjected to the correct thermal procedu.. |
|||
Tensile Strength at Break | 1140 MPa | 165000 psi | Stress relieved |
California Fine Wire Alloy 446 Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireInsulatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 1140 MPa | 165000 psi | Stress relieved |
California Fine Wire Permanickel® K-300 Nickel Alloy All values may vary dependent on specific design and usagePermanickel® is a registered trade name of the Inco family of products.Capabilities: WireRibbonInsulatedPlatedInformation provided by Calif.. |