Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 16.85 MPa | 2444 psi | AVG; ASTM D412 Method A |
Seals Eastern 5723 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 16.85 MPa | 2444 psi | ISO R 527 |
Stir SpA AF SG 85 OIL (PVC) Application: Extrusion insulation sheath CEI 20-11 type R 2 oil/petrol resistantInformation provided by STIR SpA |
|||
Tensile Strength at Break | 16.85 MPa | 2444 psi | ISO R 527 |
Stir SpA SR 80 3 (PVC) Application: Primary type TI 1Information provided by STIR SpA |