Polymer Property : Tensile Strength at Break = 1580 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.9 MPa
1580 psi
Type IV specimen; ASTM D638
LyondellBasell Petrothene® NA214000 Low Density Polyethylene
ApplicationsPETROTHENE NA 214-000 is a low density polyethylene resin specifically designed for high speed, light weight, extrusion coating applications. This resin can be drawn down to a coating w..