Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 153 MPa | 22200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific) LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength at Break | 153 MPa | 22200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36A PPS - Branched (Europe-Africa-Middle East) LNP* Lubricomp* OCL4036 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength at Break | 153 MPa | 22200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFL159 PA 66 LNP* LUBRICOMP* RFL159 is a compound based on Nylon 66 resin containing 25% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant, Flame Retardant |
|||
Tensile Strength at Break | 153 MPa | 22200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific) LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform.. |
|||
Tensile Strength at Break | 153 MPa | 22200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP EFB26ER PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EFB26ER is a compound based on Polyetherimide containing Glass Fiber, Glass Bead. Added features include: Easy Molding, Mold Release. |
|||
Tensile Strength at Break | 153 MPa | 22200 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Tensile Strength at Break | 153 MPa | 22200 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific) LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Tensile Strength at Break | 153 MPa | 22200 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP QF006 PA 6/10 LNP THERMOCOMP* QF006 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber. |
|||
Tensile Strength at Break | 153 MPa | 22200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP D551 PC (Asia Pacific) LNP* Thermocomp* D551 (or DF00A8P) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impa.. |
|||
Tensile Strength at Break | 153 MPa | 22200 psi | ASTM D638 |
Toyobo VYLOPET® EMC545 Injection Molding Polyester Resin, Glass Reinforced Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo. |