Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 15.33 MPa | 2223 psi | ASTM D638 |
LyondellBasell Alathon® M6580 High Density Polyethylene ApplicationsALATHON M 6580 is a narrow molecular weight distribution homopolymer that enhances processability and stiffness, exhibits excellent color, low odor and good processing stability. Typica.. |
|||
Tensile Strength at Break | 15.33 MPa @Temperature 200 °C, Time 252000 sec |
2224 psi @Temperature 392 °F, Time 70.0 hour |
After Dry Heat Aging; ASTM D865 |
Seals Eastern 5723 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 15.33 MPa | 2223 psi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FG 5661 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FG 5661 can be compounded using standard water cooled internal mixers or two-roll mills. The “dry” ingredients should be blended before adding to the masticated gum. .. |