Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.09 MPa | 1463 psi | AVG; ASTM D412 Method A |
Seals Eastern 7240 Ethylene-Propylene Rubber Potable water service. Chloramine resistant.Information provided by Seals Eastern, Inc. |