Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 83.4 MPa | 12100 psi | ASTM D638 |
LNP Thermocomp® JF-1004 EM M BK905 Polyethersulfone, Milled Glass Fiber
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Tensile Strength at Break | 83.4 MPa | 12100 psi | ASTM D638 |
LNP Lubricomp® PDX-E-00548 CCS Polyetherimide, Aramid Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: Lubricated, Low to None Ion ContentForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however man.. |
|||
Tensile Strength at Break | 83.4 MPa @Thickness 3.20 mm |
12100 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical Lupox® HI2152 PBT+GF15% Description: Injection Molding, PBT+GF15%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical |