Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.031 MPa | 1165 psi | Air at 302°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 121-73W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |