ExxonMobil Santoprene® 121-73W175 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 121-73W175 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall or complex profile extrusion applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion. It is polyolefin based and completely recyclable.Key Features:Recommended for applications requiring excellent flex fatigue resistance.Excellent ozone resistance.Designed for improved UV resistance.Compliant to EU Directive 2003/11/EC regarding marketing and use of certain dangerous substances and preparations, specifically pentabromodiphenyl ether or octabromodiphenyl ether.Designed for extruding thin sections with excellent definition (down to 0.33 mm [0.013"] radius). Long runs with minimal build-up of material on screen packs or narrow die sections.EU and China RoHS compliant.Applications:Automotive- Seals, Gaskets and Weather SealsUses:Automotive ApplicationsAutomotive Exterior Trim Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
Air at 302°F, 168 hr; ASTM D573
83
83
2 mm, 15 sec; ISO 868
Tensile Strength at Break 8.031 MPa
1165 psi
Air at 302°F, 168 hr; ASTM D573
8.83 MPa
1280 psi
Across Flow; ASTM D412
Tensile Stress 3.50 MPa

@Strain 100 %
508 psi

@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 450.8 %
450.8 %
Air at 302°F, 168 hr; ASTM D573
460 %
460 %
Across Flow; ASTM D412
Tear Strength 24.0 kN/m
137 pli
73°F, Die C, Across Flow; ASTM D624
Compression Set 33 %
33 %
158°F, 22 hr; ASTM D395
42 %
42 %
257°F, 70 hr; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D746
Flammability, UL94 HB

@Thickness 1.00 mm
HB

@Thickness 0.0394 in
HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Dielectric Constant 2.7
2.7
1.98 mm; ASTM D150
Dielectric Strength 27.2 kV/mm
690 kV/in
2.03 mm; ASTM D149
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Die Temperature 204 °C
400 °F
Extrusion
Melt Temperature 177 - 204 °C
350 - 400 °F
Extrusion
Drying Temperature 82.2 °C
180 °F
Dry Time 3 hour
3 hour
Back Pressure 5.00 - 20.0 MPa
725 - 2900 psi
Extrusion
Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 45
Color Black
Form Pellets