Polymer Property : Tensile Strength at Break = 1150 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 7.93 MPa
1150 psi
TM R050-36
Resinlab® EP1121-4 Adhesive / Casting Resin
Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives ..
Tensile Strength at Break 7.93 MPa
1150 psi
ASTM D638
Network Polymers NPP 11-3225
Description: Linear Low Density Polyethylene (LLDP)Information provided by Network Polymers Inc.
Tensile Strength at Break 7.93 MPa

@Temperature 23.0 °C
1150 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7680-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7680-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Tensile Strength at Break 7.93 MPa
1150 psi
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible D7500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 7.94 MPa
1150 psi
ASTM D638
LG Chemical LC370 Polyolefin Elastomer for Polymer Modification
Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio..
Tensile Strength at Break 7.93 MPa
1150 psi
Shin-Etsu Silicones KE-971TU Silicone Elastomer
KE971 TU is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding (compression, injection, transfer).P..
Tensile Strength at Break 7.93 MPa
1150 psi
ASTM D412
Teknor Apex Monprene® MP-1274G Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 7.93 MPa
1150 psi
ASTM D412
Teknor Apex Monprene® MP-2189 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 7.93 MPa
1150 psi
ASTM D412
Teknor Apex Monprene® MP-2336UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 7.92 MPa
1150 psi
ISO R 527
Stir SpA Z 2002 AT (PVC)
Application: Foamed intersoleInformation provided by STIR SpA
Tensile Strength at Break 7.93 MPa
1150 psi
ASTM D412
Teknor Apex Monprene® MP-2585B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 7.93 MPa
1150 psi
ASTM D412
Teknor Apex Telcar® TL-1431A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Strength at Break 7.93 MPa
1150 psi
ASTM D412
Teknor Apex Telcar® TL-2363H Thermoplastic Elastomer
Availability: North America Uses: Flooring; Furniture; General Purpose; Grommets; Textile Applications; Wire and Cable Applications Forms: Pellets Processing Method: Extrusion; Injection Molding In..
Tensile Strength at Break 7.93 MPa
1150 psi
ASTM D412
Teknor Apex Telcar® TL-2570A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..