Material Notes:
Application: Foamed intersoleInformation provided by STIR SpA
Physical Properties Metric English Comments
Specific Gravity 1.266 g/cc
1.266 g/cc
ISO 1183
Density 0.670 g/cc
0.0242 lb/in³
Foamed Density; ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 49
49
ISO 868
Tensile Strength at Break 7.92 MPa
1150 psi
ISO R 527
Elongation at Break 427 %
427 %
ISO R 527
Abrasion 295
295
Close, mm³; ISO 4649
810
810
Foam, mm³; ISO 4649