Polymer Property : Tensile Strength at Break = 109 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.752 MPa

@Thickness 0.127 mm
109 psi

@Thickness 0.00500 in
Tensile Lap Shear – Peak Stress; ASTM D1002-72
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Tensile Strength at Break 0.752 MPa

@Thickness 0.127 mm
109 psi

@Thickness 0.00500 in
Tensile Lap Shear – Peak Stress; ASTM D1002-72
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Tensile Strength at Break 0.752 MPa

@Thickness 0.127 mm
109 psi

@Thickness 0.00500 in
Tensile Lap Shear – Peak Stress; ASTM D1002-72
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Tensile Strength at Break 0.752 MPa

@Thickness 0.127 mm
109 psi

@Thickness 0.00500 in
Tensile Lap Shear – Peak Stress; ASTM D1002-72
3M 7952MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Tensile Strength at Break 0.752 MPa

@Thickness 0.127 mm
109 psi

@Thickness 0.00500 in
Tensile Lap Shear – Peak Stress; ASTM D1002-72
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Tensile Strength at Break 0.752 MPa

@Thickness 0.127 mm
109 psi

@Thickness 0.00500 in
Tensile Lap Shear – Peak Stress; ASTM D1002-72
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Tensile Strength at Break 0.752 MPa

@Thickness 0.127 mm
109 psi

@Thickness 0.00500 in
Tensile Lap Shear – Peak Stress; ASTM D1002-72
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Tensile Strength at Break 0.752 MPa

@Thickness 0.127 mm
109 psi

@Thickness 0.00500 in
Tensile Lap Shear – Peak Stress; ASTM D1002-72
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Tensile Strength at Break 0.752 MPa

@Thickness 0.127 mm
109 psi

@Thickness 0.00500 in
Tensile Lap Shear – Peak Stress; ASTM D1002-72
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Tensile Strength at Break 0.752 MPa

@Thickness 0.127 mm
109 psi

@Thickness 0.00500 in
Tensile Lap Shear – Peak Stress; ASTM D1002-72
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Tensile Strength at Break 0.752 MPa

@Thickness 0.127 mm
109 psi

@Thickness 0.00500 in
Tensile Lap Shear – Peak Stress; ASTM D1002-72
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Tensile Strength at Break 0.752 MPa

@Thickness 0.127 mm
109 psi

@Thickness 0.00500 in
Tensile Lap Shear – Peak Stress; ASTM D1002-72
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..