Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 0.752 MPa @Thickness 0.127 mm |
109 psi @Thickness 0.00500 in |
Tensile Lap Shear – Peak Stress; ASTM D1002-72 |
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Tensile Strength at Break | 0.752 MPa @Thickness 0.127 mm |
109 psi @Thickness 0.00500 in |
Tensile Lap Shear – Peak Stress; ASTM D1002-72 |
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Tensile Strength at Break | 0.752 MPa @Thickness 0.127 mm |
109 psi @Thickness 0.00500 in |
Tensile Lap Shear – Peak Stress; ASTM D1002-72 |
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Tensile Strength at Break | 0.752 MPa @Thickness 0.127 mm |
109 psi @Thickness 0.00500 in |
Tensile Lap Shear – Peak Stress; ASTM D1002-72 |
3M 7952MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Tensile Strength at Break | 0.752 MPa @Thickness 0.127 mm |
109 psi @Thickness 0.00500 in |
Tensile Lap Shear – Peak Stress; ASTM D1002-72 |
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Tensile Strength at Break | 0.752 MPa @Thickness 0.127 mm |
109 psi @Thickness 0.00500 in |
Tensile Lap Shear – Peak Stress; ASTM D1002-72 |
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Tensile Strength at Break | 0.752 MPa @Thickness 0.127 mm |
109 psi @Thickness 0.00500 in |
Tensile Lap Shear – Peak Stress; ASTM D1002-72 |
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Tensile Strength at Break | 0.752 MPa @Thickness 0.127 mm |
109 psi @Thickness 0.00500 in |
Tensile Lap Shear – Peak Stress; ASTM D1002-72 |
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Tensile Strength at Break | 0.752 MPa @Thickness 0.127 mm |
109 psi @Thickness 0.00500 in |
Tensile Lap Shear – Peak Stress; ASTM D1002-72 |
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Tensile Strength at Break | 0.752 MPa @Thickness 0.127 mm |
109 psi @Thickness 0.00500 in |
Tensile Lap Shear – Peak Stress; ASTM D1002-72 |
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Tensile Strength at Break | 0.752 MPa @Thickness 0.127 mm |
109 psi @Thickness 0.00500 in |
Tensile Lap Shear – Peak Stress; ASTM D1002-72 |
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Tensile Strength at Break | 0.752 MPa @Thickness 0.127 mm |
109 psi @Thickness 0.00500 in |
Tensile Lap Shear – Peak Stress; ASTM D1002-72 |
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |