Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 400 - 700 MPa | 58000 - 102000 psi | |
Goodfellow Awa®, Nickeloid®, Simlet®, Spedex® Nickel Silver Good machinability, excellent cold working and welding characteristics. Poor hot forming. Uses include rivets, screws, zippers, optical parts and costume jewelry.Information provided by Goodfello.. |
|||
Tensile Strength at Break | 550 - 700 MPa | 79800 - 102000 psi | |
ThyssenKrupp PAS 500 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |