Polymer Property : Tensile Strength at Break = 10.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.4 MPa
1510 psi
Shin-Etsu Silicones KEP-14 Silicone additive
KEP14 is an additive which can be used in most of the silicone products to neutralize acidic byproducts formed by certain peroxides and by oils at high temperatures.Product Features: Reduces peroxid..
Tensile Strength at Break 10.4 MPa
1510 psi
ISO R 527
Stir SpA C 2044 B AT (PVC)
Application: Molding for inner soleInformation provided by STIR SpA
Tensile Strength at Break 10.4 MPa
1510 psi
ISO 37
Alliance Polymers Viprene™ P80A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 10.4 MPa
1510 psi
ISO 37
Alliance Polymers Viprene™ P80A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..