Stir SpA C 2044 B AT (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Stir SpA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stir SpA C 2044 B AT (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Molding for inner soleInformation provided by STIR SpA
Physical Properties Metric English Comments
Density 1.265 g/cc
0.04570 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
ISO 868
Tensile Strength at Break 10.4 MPa
1510 psi
ISO R 527
Elongation at Break 370 %
370 %
ISO R 527
Abrasion 203
203
mm³; ISO 4649