Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1.38 - 1.72 MPa | 200 - 250 psi | |
Abatron AboSeal 8104-8 Polysulfide, Thixotropic Sealant and Caulk AboSeal 8104-8 is a 2-part, 100% solids, thixotropic polysulfide. It comes in brown, black, and other dark colors. It has been made to meet Federal Spec. TT-S-00227-E. It is an architectural standar.. |