Abatron AboSeal 8104-8 Polysulfide, Thixotropic Sealant and Caulk

Category Polymer , Adhesive , Thermoset
Manufacturer Abatron
Trade Name AboSeal
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboSeal 8104-8 Polysulfide, Thixotropic Sealant and Caulk.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboSeal 8104-8 is a 2-part, 100% solids, thixotropic polysulfide. It comes in brown, black, and other dark colors. It has been made to meet Federal Spec. TT-S-00227-E. It is an architectural standard for concrete, masonry, metal, glass, and wood. It doesn't sag on vertical surfaces. It is very soft and meets most architectural requirements.
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore A 30 - 35
30 - 35
Tensile Strength at Break 1.38 - 1.72 MPa
200 - 250 psi
Elongation at Break 300 - 350 %
300 - 350 %
Descriptive Properties Value Comments
Color Brown, Black, or other Dark Colors
Parts by Weight (pbw) 100
Part A
5
Part B