Mechanical Properties Metric English Comments
Tensile Strength at Break 0.152 MPa
22.0 psi
As manufactured
Unifrax Fiberfrax® Roll Board Ceramic Fiber Paper
The lower density, binder chemistry, and bulk ceramic fiber grade used to manufacture Fiberfrax Rollboard paper result in a product with lower cost, higher flexibility, and reduced smoke and odor du..