Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.32 J/cm
9.97 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66
LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead.