Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.99 J/cm | 7.47 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36EXP PPS - LINEAR LNP* LUBRICOMP* OCL36EXP is a compound based on Linear PPS containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include; Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Unnotched | 3.99 J/cm | 7.47 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP QL002 PA 6/10 LNP* LUBRICOMP* QL002 is a compound based on Nylon 6/10 containing 10% PTFE. Added features of this grade are: Wear Resistant. |
|||
Izod Impact, Unnotched | 3.99 J/cm | 7.47 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DEL329E PC (Asia Pacific) LNP* Stat-kon* DEL329E is a compound based on Polycarbonate resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, .. |
|||
Izod Impact, Unnotched | 3.99 J/cm @Temperature 23.0 °C |
7.47 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon OEL36A PPS LNP* Stat-Kon* OEL36A is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This .. |
|||
Izod Impact, Unnotched | 3.99 J/cm | 7.47 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |