Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 32.0 J/cm | 59.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Izod Impact, Unnotched | 32.0 J/cm | 59.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Izod Impact, Unnotched | 32.0 J/cm @Temperature 23.0 °C |
59.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® IFX2420Z PC (Asia Pacific) Lexan* IFX2420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware applications specifically for welding. This grades .. |
|||
Izod Impact, Unnotched | 32.0 J/cm | 59.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® IFX3420Z PC (Asia Pacific) Lexan* IFX3420Z is a medium viscosity, release containing, injection moldable, polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grades meets the transm.. |
|||
Izod Impact, Unnotched | 32.0 J/cm | 59.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® IFX5420Z PC (Asia Pacific) Lexan* IFX5420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grade meets the transmis.. |
|||
Izod Impact, Unnotched | 32.0 J/cm | 59.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® LUX2114 PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Izod Impact, Unnotched | 32.0 J/cm | 59.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Izod Impact, Unnotched | 32.0 J/cm | 59.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East) Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope.. |
|||
Izod Impact, Unnotched | 32.0 J/cm | 59.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® LUX2414G PC (Asia Pacific) 10 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Izod Impact, Unnotched | 32.0 J/cm | 59.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® LUX2614 PC (Asia Pacific) 7.0 MFR. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Izod Impact, Unnotched | 32.0 J/cm | 59.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Izod Impact, Unnotched | 32.0 J/cm | 59.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Europe-Africa-Middle East) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Izod Impact, Unnotched | 32.0 J/cm | 59.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |