Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.82 J/cm - NB | 10.9 ft-lb/in - NB | Average value: 10.1 J/cm Grade Count:13 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Unnotched | 5.82 J/cm @Temperature 23.0 °C |
10.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 5.82 J/cm @Temperature 23.0 °C |
10.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 5.82 J/cm @Temperature 23.0 °C |
10.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched | 5.82 J/cm | 10.9 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 611 Nylon 6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |