Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.82 J/cm - NB | 10.9 ft-lb/in - NB | Average value: 10.1 J/cm Grade Count:13 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Unnotched | 5.80 - 6.20 J/cm @Temperature 23.0 °C |
10.9 - 11.6 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RH 211/W Rigid PVC, Antishock Extrusion Various antishock profiles |
|||
Izod Impact, Unnotched | 5.80 - 6.20 J/cm @Temperature 23.0 °C |
10.9 - 11.6 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RI 528/H Rigid PVC, Antishock Injection Molding Road drains |
|||
Izod Impact, Unnotched | 5.80 - 6.20 J/cm @Temperature 23.0 °C |
10.9 - 11.6 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RKS 212/W Rigid PVC, Antishock Extrusion Lead Free Outdoor antishock profiles |
|||
Izod Impact, Unnotched | 5.80 - 6.20 J/cm @Temperature 23.0 °C |
10.9 - 11.6 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RKS 315/W Rigid PVC, Antishock Extrusion Lead Free Various profiles antishock |
|||
Izod Impact, Unnotched | 5.80 - 6.20 J/cm @Temperature 23.0 °C |
10.9 - 11.6 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RKS 325 Rigid PVC, Antishock Extrusion Lead Free Various profiles, antishock |
|||
Izod Impact, Unnotched | 5.80 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
10.9 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH720 G15 15% Glass Fiber Reinforced PC Features:Excellent balance propertiesHigh mechanical propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug partsIn.. |
|||
Izod Impact, Unnotched | 5.80 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
10.9 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH720 G20 20% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
Izod Impact, Unnotched | 5.84 J/cm | 10.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP EL002 PEI LNP* Lubricomp* EL002 is a compound based on Polyetherimide resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 5.83 J/cm | 10.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP UX96507 PPA LNP* LUBRICOMP* UX96507 is a compound based on PPA containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched | 5.80 J/cm | 10.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer LUBRICOMP* YL003C is a compound based on Polyester Elastomer resin containing 15% PTFE. Added features of this grade include: Clean Compound System, Wear Resistant. |
|||
Izod Impact, Unnotched | 5.80 J/cm | 10.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer (Asia Pacific) LUBRICOMP* YL-4030 CCS is a PTFE Lubricated Compound based on Polyester Elastomer resin which has low ionic and low outgassing performance for the Semicon and Internal Hard Disk Drive applications. |
|||
Izod Impact, Unnotched | 5.81 J/cm | 10.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP EC006PXQ PEI LNP* THERMOCOMP* EC006PXQ is a compound based on Polyetherimide containing 30% Carbon FIber. Added features include: Electrically Conductive, Easy Molding. |
|||
Izod Impact, Unnotched | 5.82 J/cm @Temperature 23.0 °C |
10.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 5.82 J/cm @Temperature 23.0 °C |
10.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 5.82 J/cm @Temperature 23.0 °C |
10.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched | 5.80 J/cm @Temperature -30.0 °C |
10.9 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Izod Impact, Unnotched | 5.80 - 6.20 J/cm @Temperature 23.0 °C |
10.9 - 11.6 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds ARC 20 Rigid PVC, Atoxic for General Purpose Bottles medium/high antishock |
|||
Izod Impact, Unnotched | 5.80 - 6.20 J/cm @Temperature 23.0 °C |
10.9 - 11.6 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds ART 20 Rigid PVC, Atoxic for General Purpose Transparent bottles medium/high antishock |
|||
Izod Impact, Unnotched | 5.80 - 6.20 J/cm @Temperature 23.0 °C |
10.9 - 11.6 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds ART 20/K1 Rigid PVC, Atoxic for General Purpose Bottles medium antishock |
|||
Izod Impact, Unnotched | 5.82 J/cm | 10.9 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 611 Nylon 6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Izod Impact, Unnotched | 5.81 J/cm | 10.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated. |