Polymer Property : Izod Impact, Unnotched = 5.59 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.59 J/cm

@Temperature 23.0 °C
10.5 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp IP003 PA6.12
LNP* Lubricomp* IP003 is a Nylon 6/12 base resin containing PTFE and Silicone.This data was supplied by SABIC-IP for the Americas region.