Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.86 J/cm | 5.36 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Izod Impact, Unnotched | 2.86 J/cm | 5.36 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched | 2.86 J/cm | 5.36 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |