Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.84 J/cm | 5.32 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX11411 PC LNP* STAT-KON* DX11411 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |