Polymer Property : Izod Impact, Unnotched = 2.84 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.84 J/cm
5.32 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DX11411 PC
LNP* STAT-KON* DX11411 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.