Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.20 - 5.30 J/cm
5.99 - 9.93 ft-lb/in
Average value: 4.26 J/cm Grade Count:3
Overview of materials for PVC, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E..