Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 25.31 J/cm | 47.42 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR6300 AES+PC+SAN (Asia Pacific) Wear resistant PC+SAN, with proprietary lubricant, for business equipment applications. |
|||
Izod Impact, Unnotched | 25.31 J/cm | 47.42 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY Lexan_WR6300 AES+PC+SAN LNP* Lubriloy* Lexan_WR6300 compound is a wear resistant PC+SAN, with proprietary lubricant, for business equipment applications. |
|||
Izod Impact, Unnotched | 25.31 J/cm | 47.42 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |