Polymer Property : Izod Impact, Unnotched = 45.32 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 24.19 J/cm
45.32 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC
LNP* LUBRICOMP* DL001 is a compound based on Polycarbonate resin containing 5% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 24.19 J/cm
45.32 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC (Asia Pacific)
LNP* Lubricomp* DL001 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated.