Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 23.54 J/cm | 44.10 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Izod Impact, Unnotched | 23.54 J/cm | 44.10 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC (Asia Pacific) LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |