Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.54 J/cm
4.76 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON OE004AE PPS - Branched
LNP STAT-KON* OE004AE is a compound based on PPS - Branched resin containing 20% Carbon Fiber. Added features of this material are: Easy Molding, Electrically Conductive.