Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.54 J/cm | 4.76 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON OE004AE PPS - Branched LNP STAT-KON* OE004AE is a compound based on PPS - Branched resin containing 20% Carbon Fiber. Added features of this material are: Easy Molding, Electrically Conductive. |