Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.34 J/cm
4.38 ft-lb/in
ASTM D412
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Izod Impact, Unnotched 2.34 J/cm
4.38 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP
LNP THERMOCOMP* MB006S is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized.
Izod Impact, Unnotched 2.34 J/cm
4.38 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF0059 PA 66
LNP THERMOCOMP* RF0059 is a compound based on Nylon 66 resin containing 25% Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
Izod Impact, Unnotched 2.34 J/cm

@Temperature 23.0 °C
4.38 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp RF0059 PA 66 (Asia Pacific)
LNP STARFLAM* RF0059 is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP for t..