Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.35 J/cm
8.15 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RBL36XXJ PA 66
LNP* LUBRICOMP* RBL36XXJ is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant.