Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.23 J/cm | 7.92 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Izod Impact, Unnotched | 4.23 J/cm | 7.92 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP MF001AS PP (Asia Pacific) LNP* Thermocomp* MF001AS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched | 4.23 J/cm | 7.92 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Izod Impact, Unnotched | 4.23 J/cm | 7.92 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Izod Impact, Unnotched | 4.23 J/cm | 7.92 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP MF001AS PP LNP* THERMOCOMP* MF001AS is a compound based on Polypropylene resin containing 5% Glass Fiber. Added features of this material include: Heat Stabilized. |