Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP MF001AS PP (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* MF001AS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.010 cm/cm

@Time 86400 sec
0.010 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 39.0 MPa
5660 psi
ASTM D638
Elongation at Break 4.9 %
4.9 %
ASTM D638
Tensile Modulus 2.28 GPa
331 ksi
50 mm/min; ASTM D638
Flexural Strength 55.0 MPa
7980 psi
ASTM D790
Flexural Modulus 2.16 GPa
313 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.23 J/cm
7.92 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C

@Thickness 3.20 mm
203 °F

@Thickness 0.126 in
unannealed; ASTM D648