Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 21.1 J/cm | 39.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY D20001 PPO LNP* LUBRILOY* Z20001 is a compound based on PPO resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant. |
|||
Izod Impact, Unnotched | 21.1 J/cm | 39.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY Z20001 PPO LNP* Lubriloy* Z20001 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant. |