Mechanical Properties Metric English Comments
Izod Impact, Unnotched 17.8 J/cm
33.3 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC
LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare.