Polymer Property : Izod Impact, Unnotched = 3.80 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.80 - 4.20 J/cm

@Temperature 23.0 °C
7.12 - 7.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RKS 218/W Rigid PVC, Antishock Extrusion Lead Free
Antishock profiles
Izod Impact, Unnotched 3.80 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
7.12 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Kingfa JH-R0G30 Flame Retardant and 30% Glass Fiber Reinforced PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood processing propertiesApplications:Injection moldingAutomobile instrument panelCD-ROM base pick-upOA device an..
Izod Impact, Unnotched 3.80 J/cm
7.12 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP ZFL31XXC PPE+PS
LNP* LUBRICOMP* ZFL31XXC is a compound based on PPE+PS resin containing 5% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant
Izod Impact, Unnotched 3.80 J/cm
7.12 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East)
VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
Izod Impact, Unnotched 3.80 J/cm

@Temperature -30.0 °C
7.12 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East)
VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
Izod Impact, Unnotched 3.80 J/cm
7.12 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East)
VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..