Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.01 J/cm
3.77 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF)
LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant.