Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.75 J/cm
7.03 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON EX11318C PEI (Asia Pacific)
LNP* Stat-Kon* EX11318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati..
Izod Impact, Unnotched 3.75 J/cm
7.03 ft-lb/in
XD; ASTM D256
DuPont™ Nomex® Type 994, 125 mil Nominal Thickness Rigid Aromatic Nylon Board
Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T..