Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.37 J/cm
6.31 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RBL36L PA 66
LNP* LUBRICOMP* RBL36L is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features s of this grade are: Low Extractable, Wear Resistant.
Izod Impact, Unnotched 3.37 J/cm
6.31 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP ZX07421 PPO
LN:* LUBRICOMP* ZX07421 is a compound based on PPO resin containing proprietary fillers. Added feature of this grade is: Wear Resistant.
Izod Impact, Unnotched 3.37 J/cm

@Temperature 23.0 °C
6.31 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp FF004 PE
LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 3.37 J/cm
6.31 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester Elastomer
LNP THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Glass Fiber, Mineral. Added features of this material include: Flame Retardant.