Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 13.72 J/cm | 25.70 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP QFL17RS PA 6/10 LNP LUBRICOMP* QFL17RS is a compound based on Nylon 6/10 resin containing 35% Glass Fiber, 5% PTFE. Added features of this material include: Easy Release, Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched | 13.72 J/cm | 25.70 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WX02869H Polyester, TP LNP THERMOCOMP* WX02869H is a compound based on Polyester, TP resin containing High Specific Gravity. Added features of this material include: High Impact. |