Mechanical Properties Metric English Comments
Izod Impact, Unnotched 13.72 J/cm
25.70 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP QFL17RS PA 6/10
LNP LUBRICOMP* QFL17RS is a compound based on Nylon 6/10 resin containing 35% Glass Fiber, 5% PTFE. Added features of this material include: Easy Release, Heat Stabilized, Wear Resistant.
Izod Impact, Unnotched 13.72 J/cm
25.70 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP WX02869H Polyester, TP
LNP THERMOCOMP* WX02869H is a compound based on Polyester, TP resin containing High Specific Gravity. Added features of this material include: High Impact.