Polymer Property : Izod Impact, Unnotched = 21.99 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 11.74 J/cm
21.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66
LNP* LUBRICOMP* RFL34 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched 11.74 J/cm
21.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 (Asia Pacific)
LNP* Lubricomp* RFL34 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 11.74 J/cm

@Temperature 23.0 °C
21.99 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Noryl PC180X PPE+PS
Nonbrominated, nonchlorinated flame retardant. V-1/5VA rated; 175F (90C) HDT. Improved productivity and reliability.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 11.74 J/cm
21.99 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 422 Heavy Mineral Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.40% Heavy Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 11.74 J/cm
21.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL PX1005X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications.